Typical applications: Mooring and tension winch mooring.
Generally: A 6 strand construction gives Atlas excellent shape retention and its elastic properties counter the need for mooring springs. Hardwearing monofilaments provide good resistance to surface abrasion. The outer filler yarns of Atlas fur up and form a shieldproviding excellent resistance to surface abrasion.
Relative density: 1,14.
Melting point: 220°C.
Shrinkage (cold water): Up to 10%.
Water uptake: Up to 10%.
UV resistance: Very good.
Abrasion resistance: Excellent.
Break elongation: Approx 28%.

  • Rope construction: 6 strand with core.
  • Material: Nylon multifilament yarn and nylon monofilaments.
  • Marking: None
  • Finish: Natural (white).

Filters